RCA CLEANGROW 5000 Å OXIDE
5000 Å SiO2
Push at 900 C in N2
Ramp to 1100 C in dry O2
Start Soak at 1090 C
Time = 48 min. in wet O2
Ramp down to 1000 C in N2
Pull at 1000 C in N2